新闻资讯
Your current location : Home >> News >> Industry News

Introduction to controllable well nitriding furnace

2019-07-17
Times

What is the controllable well type nitriding furnace?

Purpose of well type nitriding furnace:

It is mainly used for chemical heat treatment such as nitriding, nitrocarburizing and oxynitriding of various steel parts, tools and moulds and iron based powder metallurgy products. It is especially suitable for the heat treatment of aluminum profile extrusion die, and can significantly improve the service life.

真空球化退火炉.jpg

Characteristics of well type nitriding furnace:

1. The specially made, layer water-cooled seal manual patented pressing furnace cover and fan adopt a unique sealing structure, which makes the sealing more reliable. The furnace pressure can reach 3000 Pa, and the operation is convenient and labor-saving.

2. The new fan structure, integrated fan unit and diversion system make the air flow more powerful, the atmosphere flow is reasonable, and the uniformity of nitriding layer reaches ± 0.07mm, which can meet the requirements of military standard and navigation standard 2-3 furnaces.

3. Adding air blast quick cooling system can effectively shorten the production cycle.

4. The improved KRN5-W microcomputer nitrogen potential control cabinet is configured to automatically control, record and display parameters such as flow, furnace gas nitrogen potential, nitrogen decomposition rate, temperature and time according to the set program.

5. The improved KRN5-W microcomputer nitrogen potential control cabinet is configured to automatically control, record and display parameters such as flow, furnace gas nitrogen potential, nitrogen decomposition rate, temperature and time according to the set program.

6. It is equipped with a double ended dropper, which can drip organic liquid with different formulas or conduct multi gas nitrocarburizing (soft nitriding) or N-C-S multi-element nitrocarburizing by passing through the atmosphere.

7. Matched with the steam generator, it can realize steam bluing treatment of silicon steel sheets, tools and dies, and micropore filling treatment of iron based powder metallurgy parts.

8. Inject nitrogen, hydrogen and other protective atmosphere into the sealed furnace tank to conduct bright tempering or soft soldering of steel parts; Bright annealing and aging treatment of non-ferrous metals; Steel plastic deep layer hot melt composite treatment.

9. With the vacuum system, the bright heat treatment with pre vacuum protective atmosphere can be realized, and the pulse nitriding process can also be realized.

10. It can be equipped with ammonia cabinets for pressure reduction, pressure stabilization, drying, pressure, flow, ammonia decomposition rate measurement and other purposes.

11. It can be equipped with a variety of air inlet and exhaust devices to make the atmosphere in the furnace even and save 1/3 ammonia gas compared with ordinary nitriding furnace.

12. It can be equipped with a patented waste gas treatment device to achieve the goal of pollution-free emission. It is the equipment of the heat treatment plant.

The above is the relevant introduction from the well furnace manufacturer. I hope you like it.